직경: | 200mm-800mm | Ash: | 0.3% |
---|---|---|---|
Weight Of Brick: | 3-4KG/Pices | 화학적 성분: | Al2O3: 38-42%, SiO2: 50-55%, Fe2O3: 1-2% |
Installation Method: | Vibration | Transportation: | Shipping |
Keyword: | low porosity fire clay brick | Calcium Oxide Content: | ≤15% |
반열물질: | 36 | Work Temperature: | 1400C |
Crushing Strength: | 40~60 Mpa | 냉압 St: | 100분 |
Iron Content: | ≤2.0% | 냉간압쇄강도(Mpa): | 20-60 |
Material: | Fireclay | ||
강조하다: | 불에 저항 하는 불소연성 점토 벽돌,값싼 불소화 된 점토 벽돌,고온 불화성 점토 벽돌 |