제품 상세 정보:
|
| 결합 유형: | 피치 함침 | 겉보기 다공성: | 6% |
|---|---|---|---|
| MgO 함량: | 75% | 부피 밀도: | 3.01 g/cm3 |
| 차가운 분쇄 강도: | 42MPa | 하중 하에서 굴절: | 1690℃ |
| 고정 탄소 함량: | 14% | ||
| 강조하다: | C14 AOD Cone Brick,Oxidation Resistant Unit,Decarburization Vessel Lining |
||
For AOD cone section duty in a AOD refining vessel, these C14 bricks combine 75% MgO with 14% carbon and a pitch impregnated matrix that resists spalling during AOD decarburization. Carbon content is held at 14% because that is the level where thermal conductivity, slag wetting and oxidation loss stay in balance for AOD decarburization. Apparent porosity of 6% keeps liquid slag from reaching the brick interior, while a cold crushing strength of 42 MPa supports the mechanical
담당자: Mr. Pika
전화 번호: 86-13838387996
팩스: 86-0371-56010932