제품 상세 정보:
|
| 결합 유형: | 피치 함침 | 겉보기 다공성: | 6% |
|---|---|---|---|
| MgO 함량: | 78% | 부피 밀도: | 2.99g/cm3 |
| 차가운 분쇄 강도: | 45 Mpa | 하중 하에서 굴절: | 1680℃ |
| 고정 탄소 함량: | 12% | ||
| 강조하다: | C12 RH Snorkel Brick,Slag Resistant Down Leg,Vacuum Degassing Block |
||
For RH down leg snorkel duty in a RH circulation unit, these C12 bricks combine 78% MgO with 12% carbon and a pitch impregnated matrix that resists spalling during vacuum degassing. Carbon content is held at 12% because that is the level where thermal conductivity, slag wetting and oxidation loss stay in balance for vacuum degassing. Apparent porosity of 6% keeps liquid slag from reaching the brick interior, while a cold crushing strength of 45 MPa supports the mechanical
담당자: Mr. Pika
전화 번호: 86-13838387996
팩스: 86-0371-56010932